Effect of preparation methods on the metal-porcelain bond strength of Co-Cr alloys.
- Author:
	        		
		        		
		        		
			        		Jie LIU
			        		
			        		;
		        		
		        		
		        		
			        		Shuai CHI
			        		
			        		;
		        		
		        		
		        		
			        		Jin XU
			        		
			        		;
		        		
		        		
		        		
			        		Yanyan WANG
			        		
			        		;
		        		
		        		
		        		
			        		Desong ZHAN
			        		
			        		
		        		
		        		
		        		
 - Publication Type:Journal Article
 - MeSH: Alloys; Chromium Alloys; Dental Alloys; Dental Porcelain; Lasers; Materials Testing; Metal Ceramic Alloys; Metals
 - From: West China Journal of Stomatology 2014;32(2):115-118
 - CountryChina
 - Language:Chinese
 - 
		        	Abstract:
			       	
			       		
				        
				        	
OBJECTIVETo compare the shear bond strength(SBS) of cast Co-Cr alloys and selective laser melting(SLM) Co-Cr alloys with those of dental porcelain.
METHODSA dental porcelain (Vita) was applied on cast and SLM Co-Cr alloy specimens (n = 10). SBS test was conducted, and fracture mode analysis was determined. Student's t-test by SPSS 13.0 software was employed to analyze the data.
RESULTSThe SLM Co-Cr alloy specimens had lower SBS values than the cast Co-Cr alloy specimens (P > 0.05). The metal-porcelain bond strength value of the cast group was (33.11 +/- 4.98) MPa, and that of the SLM group was (30.94 +/- 5.98) MPa. The specimens in both test groups exhibited mixed failure.
CONCLUSIONThe metal-porcelain system processed by SLM exhibit a bond strength that is similar to that of the cast group. This system also display a high precision.