Study on the aging performances of fluoroelastomer FM-1D in hot air
10.16289/j.cnki.1002-0837.2025.03013
- VernacularTitle:热空气条件下氟醚橡胶FM-1D的老化性能研究
- Author:
Xiang LIU
1
;
Yi WANG
;
Yue WANG
;
Hao WU
;
Hongchang QIAN
;
Pisheng ZHAO
Author Information
1. 中国航天员科研训练中心,北京 100094
- Keywords:
fluoroelastomer;
compression set;
aging life;
compression ratio;
hot air
- From:Space Medicine & Medical Engineering
2025;36(3):259-262
- CountryChina
- Language:Chinese
-
Abstract:
To investigate the aging behavior of fluoroelastomer FM-1D in hot air,with compression set as a parameter for seal aging,aging tests were conducted on fluoroelastomer FM-1D under different initial compression rates in a hot air environment ranging from 60℃to 150℃.The aging kinetic equation relating compression set of FM-1D to temperature and time was established,in order to predict its aging life at 25℃.The test results indicated that when the initial compression rate was 30%,the compression set exhibited an Arrhenius relationship with both test temperature and time.However,at a initial compression rate of 50%,the compression set gradually conformed to the Arrhenius relationship as time extended.These findings provide a reference for determining accelerated testing methods and maintenance cycles for FM-1D rubber materials.