A study on the shear bond strength between 3D printed resin and provisional resin after thermal cycling
10.14368/jdras.2021.37.3.101
- Author:
Ji-Hun YIM
1
;
Soo-Yeon SHIN
Author Information
1. Department of Prosthodontics, College of Dentistry, Dankook University, Cheonan, Republic of Korea
- Publication Type:Original Article
- From:Journal of Dental Rehabilitation and Applied Science
2021;37(3):101-110
- CountryRepublic of Korea
- Language:English
-
Abstract:
Purpose:In this study, we intended to study the change in bond strength according to the thermal cycling of provisional resin and 3D printed resin for making provisional restoration. Materials and Methods: Through DLP method, 3D printed resin powder was used to produce 3D printed resin samples. The samples were grouped into eight groups, according to types of provisional resin (PMMA, bis-acryl resin) which is to be bonded on the samples and numbers of thermal cycling (control, 2,000, 3,000, 5,000 cycles). Shear bond strength of the bonded samples was measured on the universal testing machine.
Results:As the number of thermal cycling increased, the shear bond strength of PMMA and bis-acryl resin for 3D printed resins decreased except between 3,000 cycles and 5,000 cycles in PMMA groups. In the PMMA group, there were significant differences in shear bond strength between less number than 3,000 cycles (P < 0.05) and no significant differences between more number than 3,000 cycles (P > 0.05). In the bis-acryl resin group, there were significant differences in shear bond strength between control and 2,000 cycles, control and 3,000 cycles, and control and 5,000 cycles (P < 0.05), no significant difference between 2,000 and 3,000 cycles, between 3,000 and 5,000 cycles (P > 0.05).
Conclusion:The shear bond strength between 3D printed resin and provisional resin tended to decrease after thermal cycling.