Evaluation of the efficacy of CAD/CAM glass-ceramic onlays in molars with complicated oblique crown fracture
10.12016/j.issn.2096-1456.2019.12.005
- Author:
FENG Ermei
1
;
ZHANG Yanxia
2
Author Information
1. Department of Endodontics, Stomatological Hospital,Southern Medical University
2. Department of Stomatology , The First Hospitai of Shi Jiang Zhuang City
- Publication Type:Journal Article
- Keywords:
CAD/CAM;
glass-ceramic;
onlays;
all ceramic crown;
molars;
crown and root fracture;
sulcus bleeding index;
plaque index;
gingival index
- From:
Journal of Prevention and Treatment for Stomatological Diseases
2019;27(12):775-778
- CountryChina
- Language:Chinese
-
Abstract:
Objective:To evaluate the clinical efficacy of CAD/CAM glass-ceramic onlays in molars with complicated oblique crown fracture within 3.0 mm subgingival.
Methods:Fifty-six molars from 56 patients with complicated oblique crown fracture within 3.0 mm subgingival were recruited after endodontic treatment and divided into 2 groups according to the restorative methods used. The glass-ceramic onlays group was restored with CAD/CAM glass-ceramic onlays, while the all-ceramic crown group received CAD/CAM all-ceramic crowns. The success rates of the restorations were analyzed, and the sulcus bleeding index (SBI), plaque index (PLI), and gingival index (GI) were recorded at the prerestoration and postrestoration stages.
Results :After one year of follow-up, the success rate of the glass-ceramic onlay group was 96.4%, and the success rate of the all-ceramic crown group was 92.9%. The difference was not statistically significant (P > 0.05). No differences in SBI, PLI, or GI were found between the glass-ceramic onlay group and the all-ceramic crown group (P > 0.05).
Conclusion:Conclusion