Experimental mechanics analysis of posterior galvano-ceramic bridges made by Ni-Cr pontic fired bonding galvano caps
- VernacularTitle:后牙金沉积内冠熔结镍铬桥体烤瓷桥的实验力学分析
- Author:
Tuanfeng ZHOU
;
Xinzhi WANG
;
Guirong ZHANG
;
Feng SUN
- Publication Type:Journal Article
- Keywords:
Metal ceramic alloys;
Dental abutments;
Dental stress analysis;
Gold alloys;
Chromium alloys
- From:
Journal of Peking University(Health Sciences)
2004;0(01):-
- CountryChina
- Language:Chinese
-
Abstract:
Objective: To measure the fracture strength of the posterior galvano-ceramic bridges made by Ni-Cr pontic fired bonding galvano caps with highly temperature-resistant adhesive and to provide re-ference data for clinical application. Methods: A standard low dental cast was achieved with 46 missing. Five posterior galvano-ceramic bridges made by Ni-Cr pontic fired bonding galvano caps, with abutments being 47 and 45 . The low dental cast was fixed on the panel of the universal testing machine, vertical load given on the central of the pontic as the velocity of 2 mm/min. Results: The fracture strength of the posterior galvano-ceramic bridges made by Ni-Cr pontic fired bonding galvano caps was (877.00?126.53) N, the fracture strength of the metal frame was (1 448.94?51.02) N. Conclusion: Posterior galvano-ceramic bridges made by Ni-Cr pontic fired bonding galvano caps could endure the normal human occlusal force.