The influences of repeated firing cycle on the color of the glass/alumina composite -veneering porcelain structure
- VernacularTitle:反复烧烤对渗透陶瓷—面瓷复合体颜色的影响
- Author:
Yukun MENG
;
Yonglie CHAO
;
Yunmao LIAO
- Publication Type:Journal Article
- Keywords:
Dental firing;
Glass/alumina composite;
Veneering porcelain;
Color
- From:
Journal of Practical Stomatology
1996;0(02):-
- CountryChina
- Language:Chinese
-
Abstract:
0.05). The maximum color differences ( ?E) in the selected firing cycles were 2.279 8 and 1.389 4 for GI Ⅱand Vita In Ceram Alumina groups respectively, the maximum ?E between the two groups was 2.295 6, which fell into the clinically acceptable threshold for color differences. Conclusion: Color stability of all ceramic restorations with GI Ⅱand Vita In Ceram Alumina as substructure can be guaranteed after repeated firing of veneering porcelain up to 10 times.