The effect of different pore sized hydroxyapatite for promoting bone vascularization in tissue engineering
10.3969/j.issn.1671-8348.2015.23.008
- VernacularTitle:不同孔径的羟基磷灰石对组织工程骨血管化促进效果的研究
- Author:
Guozhi YANG
;
Changcheng ZHANG
;
Zhenwu LI
;
Ruiqiang ZHAO
;
Junting LIU
;
Ruifeng YIN
;
Zhian LI
- Publication Type:Journal Article
- Keywords:
hydroxyapatites;
neovascularization,physiologic;
tissue-engineered bone;
bone defect
- From:
Chongqing Medicine
2015;(23):3195-3197
- CountryChina
- Language:Chinese
-
Abstract:
Objective To investigate the effect of different pore sized hydroxyapatite for promoting bone vascularization in tissue engineering.Methods Male Wistar rats were randomly divided into three groups,named group A,B and C,which were im-planted hydroxyapatite bioceramics compositing 4 μg bone morphogenetic protein with different aperture of 200 -300,350 -450, 500-600 μm in the back subcutaneously.The size of each block was 5 mm×5 mm×1 mm in a weight about of 40.0 mg.After im-plantation,the animals were killed and the implants and the surrounding tissue were taken out at the first,second,third and forth week respectively.HE staining of histological analysis was used to detect the situation of local neovascularization.Results There was significant difference between second and third week in group A.Comparing the area of vascularization at different time points in group B and group C,there were significant difference in the comparison of intragroup (P <0.05 ).During the first week after surgery,there was only group C that had the area of vascularization.During the second and forth week after operation,the area of vascularization in group B and group C were significant higher than group A (P <0.05).The C group showed a great deal of new-born blood vessels and clear formation of bone trabeculae.Conclusion The hydroxyapatite bioceramics of 500-600 μm could better promote vascalarization of tissue engineering in bone.