Effects of three bond agents on bond strength of titanium- ceramic system
10.3969/j.issn.1001-3733.2010.02.05
- VernacularTitle:3种粘接瓷对钛瓷结合强度的影响
- Author:
Fei TAN
;
Yumei ZHANG
;
Ruobing ZHANG
;
Shaopeng QI
- Publication Type:Journal Article
- Keywords:
Bond agent;
Titanium;
Porcelain;
Bond strength
- From:
Journal of Practical Stomatology
2010;26(2):160-164
- CountryChina
- Language:Chinese
-
Abstract:
Objective:To evaluate the effects of three bond agents on bond strength of titanium- ceramic system. Methods: The pure titanium specimens were randomly divided into three groups. Three different manufacturers' porcelains(Super Ti22,Duceratin,Titankeramik) were used specially for titanium- ceramic bonding. The specimens in each group were further divided into two subgroups:bond agent group and no bond agent group. Bond strength of specimens was measured by the three- point bending test according to ISO9693. The titanium- ceramic interfaces were investigated by SEM/EDS. Results:The bond strength of Super Ti22(35.84±2.17) MPa and Duceratin(35.45±2.37) MPa with bond agent group was significantly higher than that of no bond agent group(P<0.05). Titankeramik with bond agent group showed a little higher bond strength than without bond agent, but no significant difference in statistics(P>0.05). The interfaces of Super Ti22 and Duceratin with bond agent groups were compact, while there were visible cracks and pores at the interface of other groups. Conclusion:The application of bond agent can improve bond strength of titanium- ceramic system.