Effect of ferrule on the fracture resistance of mandibular premolars with prefabricated posts and cores.
- Author:
Ae Ra KIM
1
;
Hyun Pil LIM
;
Hong So YANG
;
Sang Won PARK
Author Information
- Publication Type:Original Article
- Keywords: Ferrule; Mandibular premolar; Fracture resistance; Post
- MeSH: Bicuspid*; Crowns; Tooth
- From:The Journal of Advanced Prosthodontics 2017;9(5):328-334
- CountryRepublic of Korea
- Language:English
- Abstract: PURPOSE: This study evaluated fracture resistance with regard to ferrule lengths and post reinforcement on endodontically treated mandibular premolars incorporating a prefabricated post and resin core. MATERIALS AND METHODS: One hundred extracted mandibular premolars were randomly divided into 5 groups (n=20): intact teeth (NR); endodontically treated teeth (ETT) without post (NP); ETT restored with a prefabricated post with ferrule lengths of either 0 mm (F0), 1 mm (F1), or 2 mm (F2). Prepared teeth were restored with metal crowns. A thermal cycling test was performed for 1,000 cycles. Loading was applied at an angle of 135 degrees to the axis of the tooth using a universal testing machine with a crosshead speed of 2.54 mm/min. Fracture loads were analyzed by one-way ANOVA and Tukey HSD test using a statistical program (α=.05). RESULTS: There were statistical differences in fracture loads among groups (P<.001). The fracture load of F2 (237.7 ± 83.4) was significantly higher than those of NP (155.6 ± 74.3 N), F0 (98.8 ± 43.3 N), and F1 (152.8 ± 78.5 N) (P=.011, P<.001, and P=.008, respectively). CONCLUSION: Fracture resistance of ETT depends on the length of the ferrule, as shown by the significantly increased fracture resistance in the 2 mm ferrule group (F2) compared to the groups with shorter ferrule lengths (F0, F1) and without post (NP).